selectivity between silicon nitride and silicon
2002-03-07
Roger Shile
selectivity between silicon nitride and silicon
Roger Shile
2002-03-07
SiO2 would probably provide a better mask, but if you don't need to etch very
deep the nitride might suffice.  Better yet if you have resist on top of the
nitride as extra protection.  SF6 is an excellent etchant for Si using RIE.

Roger Shile

>>> [email protected] 03/07/02 09:33AM >>>
Hi,
I am going to etch silicon using silicon nitride as the mask. But I only
have CF4, SF6, O2 and He... I am not sure if those gases are enough for my
application or I need to order some new gases.
Thanks.

Peng Yao
DOEs lab
Electrical Engineering Dept.
Univeristy of delaware
Newark D.E 19716
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Mentor Graphics Corporation
University Wafer