A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: how to etch SiO2 with RIE
how to etch SiO2 with RIE
2002-03-06
Peng Yao
2002-03-07
Roger Shile
2002-03-07
[email protected]
2002-03-08
Stefan Wiechmann
2002-03-14
Ravi Shankar
2002-03-07
Peng Yao
2002-03-08
[email protected]
2002-03-08
[email protected]
how to etch SiO2 with RIE
Peng Yao
2002-03-07
Hi Bob,
I am using PhotoResist as the mask during etching. And the thickness I
want is about 1.5 micron. Actually, I want etch both the photoresist and
the SiO2 at the same etching rate, so that I can transfer the gray scale
structure of my photoresist to SiO2. I have tried using CF4+O2, but my
glass sample was really tough to be get rid of. I am thinking one of the
possible reason is that the glass sample I used, which is actrually used
as microscope cover... Maybe I have to buy some silica wafer to do this
work.


Peng Yao
DOEs lab
Electrical Engineering Dept.
Univeristy of delaware
Newark D.E 19716

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.