Ravi Shankar
2002-03-07
Peng Yao
2002-03-08
[email protected]
2002-03-08
[email protected]
how to etch SiO2 with RIE
[email protected]
2002-03-08
What you are trying to do is difficult. You will need to establish a 1:1 etch
rate oxide vs. photoresist. This will require a ratio around 50% CF4  50% O2.
Do you have instruments available to measure these films. Probably a Dektac
surface scanning system will work. Also I would recommend using a larger
substrate as cooling on the electrode becomes important during the etch
cycle. Bob

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group
MEMS Technology Review