How to remove residual SiNx ?
[email protected]
2002-03-14
rie etch with SF6 should do the trick. Try 250 millitorr as a partial
pressure using the mass flow controller to get to that pressure. Should be
around 40 sccm of SF6 gas. Power level of 150 watts with a reflective of <10
watts should give descent uniformity of Nitride etch. Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review