How to get 2" Si wafer and etch 45 degree V-groove?
2002-03-18
lib zhou
How to get 2" Si wafer and etch 45 degree V-groove?
2002-03-19
Kenneth Smith
How to get 2" Si wafer and etch 45 degree V-groove?
lib zhou
2002-03-18
Hi,Dear All:

I am interested to know if anyone can send me some information which company
can still sell high quality 2" single-crystal silicon wafer. by the way, I have
an another
question related to (100) Si anisotropic etch by KOH, how can get a 45 (or
135)degree  bevel plane at the end of a V-groove, this angle refer to the
inclination of the end bevel plane to the V-groove axes line (or bottom line). I
think the method cuting (100) silicon at 9.7 degree angle can only get the bevel
plane have a 45degree to Si surface, the angle between the bevel plane and the
V-groove bottom line is still -54.7 degree.


Thanks ahead and best regards,

Lib Zhou
Yahoo! Sports - live college hoops coverage

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics