any plasma treatment should render the surface hydrophilic.  This means you
can plasma treat with inert gas, say argon and not etch to much of the
original material but create a hydrophilic surface.  Bill Moffat

-----Original Message-----
From: Xinyu Li [mailto:[email protected]]
Sent: Wednesday, March 20, 2002 1:14 PM
To: [email protected]
Subject: [mems-talk] Changing PDMS surface from hydrophobic into
hydrophilic


Dear colleagues,

Besides using oxygen plasma treat PDMS surface, are there any other ways
to change it from hydrophobic into hydrophilic?

Thanks.

Xinyu Li, PhD
Senior Scientist
Bioprocessors
35-C Cabot Road
Woburn, MA 01801
Tel: (781)935-1400 ext. 18
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group
Mentor Graphics Corporation