MEMSnet Home: MEMS-Talk: Cr/Cu wet etching
Cr/Cu wet etching
2002-03-29
Jai Shinh
2002-04-01
Bill Moffat
Cr/Cu wet etching
Jai Shinh
2002-03-29
Hello,

Could anyone help me to solve the problem of wet etching Cr/Cu?  The copper is
on top of the chrome.

I have a hard time protecting the copper when etching the chrome.

For chrome etchants, I've tried 1020 AC from the Transene, and CR-4.

The pattern is 40 microns in width, and Cr/Cu is 100 A/ 1 um.  The undercut is
severe.

Any suggestions will be greatly appreciated.



Regards,

Jai
Yahoo! Greetings - send greetings for Easter,  Passover

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer