>Has anyone ever anodically bonded pyrex to both sides?  All the
literature
>I read only describes the process for one side.

You can check:
M. Despont et al, "Fabrication of a silicon-Pyrex-silicon stack by A.c.
anodic bonding",
Sensors and Actuators A55 (1996), pp. 219-224.



Adriana Lapadatu, Ph.D.
Technology Development

SensoNor asa
Knudsrxdveien 7
P.O.Box 196
N-3192 Horten
Norway

tel: +47 33 03 50 79
Fax: +47 33 03 51 05

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing