PECVD process
2002-04-10
Liz Shelley
I Need SOI
2002-04-10
Rick Williston
2002-04-11
Vic Kley
2002-04-12
Rick Williston
PECVD process
Liz Shelley
2002-04-10
I'm depositing a 1.2-1.3 micron  PECVD oxide layer with a
Plasma Therm  ETP-3       I am getting excellent uniformity and
rate of 200 angs/min OCCASIONALLY.  Then the rate and
uniformity gradually or abruptly goes to hell.

Question: what is the order of influence of each variable?
ie Temperature of pallet       (250C)
   Process pressure             (600mTorr)
   Power                               (20W)
   N2 flow                            (600sccm)
   N2O flow                          (600sccm)
   5% SiH4 flow                    (630sccm)
Any information or direction is gratefully appreciated.
Liz

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
MEMStaff Inc.
The Branford Group