Wet Etching
Amit Shiwalkar
2002-04-11
Hello,

500 um is a hugh depth, I dont know what is your feature size. SiO2 will
not withstand KOH and there are problems even with TMAH. My suggestion is
that you use Ethylene Diamine + Pyrocatechol mixture, where SiO2 will serve
as an effective etch mask.

Regards
Amit Shiwalkar

aslam muhammad wrote:

> Hi Friends
>
>               I want to use TMAH and KOH as etchant to
> etch bulk silicon ( 500 micron).  which one is more
> suitable.  my etch mask is SiO2.  what is the recipe
> of a good etching rate KOH and TMAH please.
>
> Thankx
>
> M. Aslam




"Your reality is a figment of my Imagination"
      ......... To me you exist because I imagine that you do.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing