MEMSnet Home: MEMS-Talk: HOW to remove OTS SAM on silicon layer??
HOW to remove OTS SAM on silicon layer??
2002-04-10
양지철
2002-04-12
Jens Tuchscheerer
HOW to remove OTS SAM on silicon layer??
Jens Tuchscheerer
2002-04-12
Hi,
...you can try a buffererd HF. The result can you check by measurment the
contact-angle.
Jens Tuchscheerer



----- Original Message -----
From: ">gAvC6" 
To: 
Sent: Thursday, April 11, 2002 5:48 AM
Subject: [mems-talk] HOW to remove OTS SAM on silicon layer??


> I want to get rid of OTS ( Octadecyltrichlorosilane ) coating layer on
silicon sub.
>
> Specially, I want to know which chemical can remove the OTS SAM.
>
> If you have any suggestion, It's very thanksful for me.
>
> ****
> Nano-Tribology Research Lab.Yonsei University, Korea.
>  Ji Chul Yang
>
>  [email protected]
>
>   Have a nice day.
> *****
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.
Mentor Graphics Corporation