Hi,

I am looking for a coating that prevents protein adsoption on a PDMS
microchannels. This coating needs to last at least 3 months without coming off.
I will appreciate any advice.

thanks a lot!
Gabriela

Gabriela Juarez-Martinez
Dept. Electronics
Rankine Building
University of Glasgow
Glasgow G12 8LT, UK.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Mentor Graphics Corporation
Nano-Master, Inc.