    I am trying to pattern a thick silver layer on GaAs. The thickness could
be 5000A to 1um . The pattern I try to make is a 30X20um rectanglular
openning. I once tried the silver etchant from Transene. It gave me huge
undercut and ugly etch front. Anyone has the similar problem before? I
deposit silver in CHA E-beam deposition system at about 3~5A/sec.
   Is it OK to lift off this pattern in suck a thick layer? As I know, it is
normally more difficult to lift off a small openning than a mesa or ridge.
   Anther question is, I am using AZ5214, and AZ4330 now. will the image
reversal give these PR a better profile for lift off? Will the Chlorobenzene
process or toluene work to them too?

  Thanks a lot for your help
   Qingwei

**********************************************************
Mo, Qingwei                                              *
Phone:(512)-476-4746 (H)                                 *
      (512)-471-7917 (O)                                 *
Fax:  (512)-471-8575 (O)                                 *
Email: [email protected], [email protected]              *
                                                         *
/------   \ | | /  ---------------------\                *
|          -----       | |Microelectronic Research Center*
|        [  @ @  ]      | Electrical and Computer Eng.   *
\--oOOO-----(_)----OO0o-| University of Texas at Austin  *
**********************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics