MEMSnet Home: MEMS-Talk: Teflon AF Adhesion Problem
Teflon AF Adhesion Problem
2002-04-19
Rishi Mulgund
2002-04-22
Mighty Platypus
2002-04-23
Jens Tuchscheerer
How to calculate the effective dielectric constant?
2002-04-24
JIAO JW
SU8 resistivity
2002-05-10
Mihaela Balseanu
Teflon AF Adhesion Problem
Mighty Platypus
2002-04-22
We use HMDS, and it works pretty well. We've found that borosilicate float
glass works better than pyrex in terms of spin-coating. What kind of glass
are you using?

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Battery is safe if not provoked." -- _Batteries in a Portable World_

On Fri, 19 Apr 2002, Rishi Mulgund wrote:

> Hello All,
>       I am trying to Spin Coat Teflon AF 2400 onto a glass substrate but I am
> having problems getting the Teflon to uniformly coat because of adhesion
> problems.  I have heard a great deal of talk about using fluorosilane as an
> adhesion agent, but I can't seem to find it anywhere.  Does anyone know
> where I might be able to find this fluorosilane or have any possible
> solutions to my adhesion problem?
>
> Rishi Mulgund
>
> __________________________________________________
> Rishi D. Mulgund
> [email protected]
> (716) 274-4293
> CPU Box 273662
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing