Convex Corner Compensation
2002-04-22
Michele Finardi
2002-04-22
Mighty Platypus
2002-04-23
Dongil (Dan) Cho
2002-04-22
Roger Shile
2002-04-23
BERAUER,FRANK (HP-Singapore,ex7)
Convex Corner Compensation
Mighty Platypus
2002-04-22
References for corner compensation:

X.P. Wu and W.-H. Ko, "A study on Compensating Corner Undercutting in
Anisotropic Etching of (100) Silicon," Transducers '87, pp. 126-9.

H. Sandmaier, H.L. Offereins, K Ku:hl, and W. Lang, "Corner Compensation
Techniques in Anisotropic Etching of (100) Silicon Using Aqueous
KOH," Transducers '91, pp. 456-9.

P. Enoksson, G. Stemme, and E. Stemme, "Vibration Modes of a Silicon Tube
Density Sensor," JMEMS V.5, #1, pp. 39-44.

P. Enoksson, "New Structure for Corner Compensation in Anisotropic KOH
Etching," JMEMS V.7, #3, pp. 141-4.

The source I got these from is pretty old, so it doesn't give anything
newer than about 1998.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Battery is safe if not provoked." -- _Batteries in a Portable World_

On Mon, 22 Apr 2002, [iso-8859-1] Michele Finardi wrote:

> Hallo,
> I'm about to start working on convex corner
> compensation. Could you please indicate me some
> references or share your personal knowledge?
> Thank you very much.
>
> Michele Finardi
>
> ______________________________________________________________________
> Vinci i Mondiali - La Grande Sfida dei Mondiali FIFA
> http://it.yahoo.com/mail_it/foot/?http://lasfida.yahoo.net/
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group