MEMSnet Home: MEMS-Talk: Wet etch of SOI
Wet etch of SOI
2002-04-20
Peng Yao
2002-04-22
Mighty Platypus
2002-04-23
Peng Yao
2002-04-24
Mighty Platypus
2002-04-26
Ravi Shankar
2002-04-24
[email protected]
Plasma etch of BCB
2002-04-24
Lester Lopez
Wet etch of SOI
Mighty Platypus
2002-04-24
According to "Etch Rates for Micromachining Processing" (JMEMS V.5,#4) it
will not attack single crystal silicon

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Battery is safe if not provoked." -- _Batteries in a Portable World_

On Tue, 23 Apr 2002, Peng Yao wrote:

> Hi Jesse,
> Will phosphoric acid attack Silicon as well?
> Thanks
>
> Peng Yao
> DOEs lab
> Electrical Engineering Dept.
> Univeristy of delaware
> Newark D.E 19716
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.
Nano-Master, Inc.