MEMSnet Home: MEMS-Talk: Wet etch of SOI
Wet etch of SOI
2002-04-20
Peng Yao
2002-04-22
Mighty Platypus
2002-04-23
Peng Yao
2002-04-24
Mighty Platypus
2002-04-26
Ravi Shankar
2002-04-24
[email protected]
Plasma etch of BCB
2002-04-24
Lester Lopez
Wet etch of SOI
Ravi Shankar
2002-04-26
no phosphoric acid does not attack silicon to a great amount
Regds
Ravi Shankar
Semiconductor Complex Ltd
India


On Tue, 23 Apr 2002, Peng Yao wrote:

> Hi Jesse,
> Will phosphoric acid attack Silicon as well?
> Thanks
>
> Peng Yao
> DOEs lab
> Electrical Engineering Dept.
> Univeristy of delaware
> Newark D.E 19716
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review
University Wafer