MEMSnet Home: MEMS-Talk: Lamda Router micromirror
Photomasks for Mems
2002-04-24
[email protected]
Lamda Router micromirror
2002-04-26
sou zou
Lamda Router micromirror for optical switches
2002-04-30
sou zou
Lamda Router micromirror
sou zou
2002-04-26
 Hi mems-talk members,
I am wondering if someone knows about the process flow, the technology
(mterials, deposition methods, ...), or any reliable informations (papers, Web
sites) about the design of this successfull MOEM device, which is difficult or
may be impossible to make under some typical processes like MUMP's or SOI-based
process-flows. In fact, the only informations I got through the web includes
only some technical informations and advertisement stuffs.
Any help would be very gratefull and thanks in advance everyone.
sz



---------------------------------
Yahoo! Mail -- Une adresse @yahoo.fr gratuite et en frangais !

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Harrick Plasma, Inc.
Nano-Master, Inc.