MEMSnet Home: MEMS-Talk: Problem in applying Voltage across Pt
Problem in applying Voltage across Pt
2002-04-27
Chan Ho Yin
2002-04-29
Mighty Platypus
2002-04-30
Chan Ho Yin
Problem in applying Voltage across Pt
Chan Ho Yin
2002-04-30
Hi Mighty Platypus,

    Thank you for your help first. Yes. I put the cantilever beam
underwater.  And the cantilever is made of polymer and Pt (2 layers).
First deposit polymer and then Pt. And it is surely a free standing beam.


    Then, it means that we can't avoid the bubbles?

Yours,
Hoyin


>From: Mighty Platypus 
>Reply-To: [email protected]
>To: [email protected]
>Subject: Re: [mems-talk] Problem in applying Voltage across Pt
>Date: Mon, 29 Apr 2002 09:41:18 -0700 (PDT)
>
>Chan Ho Yin,
>I think your problem needs a little more description. First, is your
>device a platinum cantilever beam directly deposited on a silicon
>substrate, with no other layers?
>Second, it reads as if you are sticking two probes (of unknown
>material) on to a platinum wire, with nothing else between them. There is
>no mention of what kind of atmosphere they have been placed in. But,
>electroysis makes me think of water. So, what are the probes made of, what
>kind of circuit do they form, and are they in air, water, or something
>else?
>
>If it turns out you have naked wires in water, then you'll definitely have
>electrolysis, even at relatively low voltages.
>
>Jesse Fowler
>   UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
>   Los Angeles, CA 90095-1597 | (310)825-3977
>"Battery is safe if not provoked." -- _Batteries in a Portable World_
>----- BEGIN GEEK CODE BLOCK -----
>Version 3.1
>GE/S$ d- s:- a- C+ UL P L++ E- W+ N+@ !o K++ w !O M !V PS+ PE++(-) Y
>PGP-- t++@ 5++ X R+ !tv b++ DI+ D G e++/*>++++/* h---/* r+++ y+++
>------ END GEEK CODE BLOCK ------
>
>
>On Sat, 27 Apr 2002, Chan Ho Yin wrote:
>
> > Hi all,
> >
> >     I have deposited Pt onto Si substrate and make Pt into a line. When
I
> > applied DC voltage to its two ends by micro probes, I found that there
are
> > many bubbles come out from the contact point between the probes and Pt
> > layer.  I guess it dues to electrolysis. I also applied AC to it.. But
> > still many bubbles...
> >
> >    What is the problem??  Can I reduce the bubbles or stop the bubbles
> > generated??  Can you suggest me some methods??????????
> >
> >   By the way, the structure is a cantilever beam.  (2 layers).
> >
> > Thank you.
> >
> > Yours,
> > Hoyin
> >
> > _________________________________________________________________
> > &b1z*:&f0J8K8m$W6G0e15&, Hotmail 6l%s!A=P2>&\!Ghttp://mobile.msn.com
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.mems-exchange.org/
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/


_________________________________________________________________
&b1z*:&f0J8K8m$W6G0e15&, Hotmail 6l%s!A=P2>&\!Ghttp://mobile.msn.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation