Contact Angles of Semiconductor Films
2002-05-03
Tariq M. Haniff
2002-05-06
Bill Moffat
Contact Angles of Semiconductor Films
Bill Moffat
2002-05-06
Tariq,
      I have personally worked on a number of papers that discuss contact
angles for semiconductor processing.  I am just down the road, close to the
Milpitas border and would like to discuss with you the action of plasma and
silanes as contact angle control processes. Having manufactured HMDS primers
for over 20 years and plasma surface modifiers for over 15 years we have lots
of experience with contact angle measurement.  Bill Moffat  408 954 8353

-----Original Message-----
From: Tariq M. Haniff [mailto:[email protected]]
Sent: Friday, May 03, 2002 11:14 AM
To: [email protected]
Subject: [mems-talk] Contact Angles of Semiconductor Films


Dear Members,

I am looking for a good summary of hydrophobicity/hydrophilicity of films
compatible with semiconductor processing.
Films like, thermal oxide, LTO, BPSG, Si3N4, etc. Specific contact angle
would
be great. Can anyone point me in the right direction?

Thanks in advance,

Tariq M. Haniff
Genospectra, Inc
6519 Dumbarton Circle
Fremont, CA 94555
510-818-2600
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing