Au-Sn solder
Phil
2002-05-09
Adnan,

We are working on optical packaging systems and have some experience in
producing this type of solder.  You can call me at (562) 437-0541 and we can
discuss your application in more detail.

Phil Stapleton

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of adnan merhaba
Sent: Wednesday, May 08, 2002 7:45 AM
To: [email protected]
Subject: [mems-talk] Au-Sn solder


hello all,

does anyone have any experiences with plating Au-Sn
(80-20) solder alloy, or any other viable means of
depositing the same (apart from screen-printing,
sputtering and evaporation), or is there any available
literature on the same.

I am looking to plate/deposit Au-Sn on pads of various
sizes ranging from 100x100 mils to 20x20 mils,
thickness ranging from 5 micron to 50 microns.

Thanking you in anticipation.
Regards,
Adnan
Yahoo! Health - your guide to health and wellness
http://health.yahoo.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

[demime 0.98e removed an attachment of type application/ms-tnef which had a name
of winmail.dat]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation