MEMSnet Home: MEMS-Talk: Teflon coating
Teflon coating
2002-05-13
Xuchun Liu
2002-05-14
Mighty Platypus
2002-05-14
[email protected]
Teflon coating
Mighty Platypus
2002-05-14
Spin-coatable teflon is known as Teflon AF. It is available from DuPont
only.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Battery is safe if not provoked." -- _Batteries in a Portable World_
----- BEGIN GEEK CODE BLOCK -----
Version 3.1
GE/S$ d- s:- a- C+ UL P L++ E- W+ N+@ !o K++ w !O M !V PS+ PE++(-) Y
PGP-- t++@ 5++ X R+ !tv b++ DI+ D G e++/*>++++/* h---/* r+++ y+++
------ END GEEK CODE BLOCK ------


On Mon, 13 May 2002, Xuchun Liu wrote:

> Hello, everyone,
>
> Does anyone have experience on teflon spin-coating
> before? I just wonder what product it is and what is
> the name of the vender in US. Thank you very much in
> advance!
>
> Bert
> LAUNCH - Your Yahoo! Music Experience
> http://launch.yahoo.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group