A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: mems-talk digest, Vol 1 #291 - 7 msgs
RE: mems-talk digest, Vol 1 #291 - 7 msgs
2002-05-20
Marc Straub
RE: Gold film
2002-05-22
Marc Straub
2002-05-22
Joyce Wong
2002-05-24
Gurvinderjit Singh
RE: mems-talk digest, Vol 1 #291 - 7 msgs
Marc Straub
2002-05-20
Gurvinderjit,

I suspect that your film is "beading" like water on a waxed surface and
forming into discrete gold islands.  Gold does not wet or adhere to oxides
well, particularly in very thin layers.  Heating the surface gives the Au
atoms the energy they need to migrate.

Depending upon your application, you should try a thicker layer and/or
flashes (thin layers) of Cr/Cu, Ti or Ti/W under the Au for better adhesion.
Good luck.

--
Marc Straub
Staff Engineer, Product Development Services
Coventor, Inc.  (Formerly Microcosm Technologies)
7 Corporate Park, Suite 260
Irvine, CA  92606
Ph: 949-756-0033  Fax: 949-756-0070
[email protected]  [remove the "XXXX"]


> -----Original Message-----
> Date: Mon, 20 May 2002 11:20:15 +0530 (IST)
> From: Gurvinderjit Singh 
> To: [email protected]
> Subject: [mems-talk] Gold film
> Reply-To: [email protected]
>
> Dear friend i have one query.
> I am depositing gold film (thickness 0.1 micron)by thermal evaporation on
> oxides,
> but when  i am annealing my sample to 700K this gold film become non
> -conductive may be  duo to formation of gold oxide. But from
> literature i found
> that gold should not become oxide till 1200K. I also read people using
> gold electrodes (thin film by thermal evaporation) on their samples and
> work till 900k kindly let me know where i am doing mistake, wether to take
> more thick film or something else.
>
>
>
> __________________________________________________________________
> _____________
>
>
>    Gurvinderjit Singh Ahluwalia             Tel: +91-0731-488656
>      Laser Materials Division               Fax: +91-0731-488650
>    Centre for Advanced Technology         email: [email protected]
>    Indore - 452 013  INDIA

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering