MEMSnet Home: MEMS-Talk: Highest resistivity silicon?
Highest resistivity silicon?
2002-05-20
Fred Hussain
2002-05-20
Michael Pedersen
2002-05-20
David Nemeth
2002-05-20
Michael Barger
2002-05-20
Kenneth Smith
2002-05-22
mmf
2002-05-20
Kenneth Smith
2002-05-20
Michael D Martin
Highest resistivity silicon?
mmf
2002-05-22
Dear Fred,

If your design allows, you could use 1000 ohm.cm silicon, Lithium
drift it, which would compensate the carriers, thereby raising the
resistivity to the equivalent of 25kohm.cm at low temperature. It is
a well known technique for producing large depleted volumes in
silicon for nuclear particle detectors.

mateen






> -----Original Message-----
> From: [email protected] [mailto:[email protected]]On
> Behalf Of Fred Hussain
> Sent: Monday, May 20, 2002 6:47 AM
> To: [email protected]
> Subject: [mems-talk] Highest resistivity silicon?
>
>
> Dear all,
>
> I am looking for silicon substrates which can be machined using conventional
> MEMS type processes, but at the same time are highly insulating. I've found
> a web page with silicon of 250Kohm-cm resistivity -
> http://www.tydex.ru/materials/materials2/Si.html.
>
> Does anybody:
> have any experience of working with such materials?
> know of any issues, for example the stability of the resistivity with
> temperature?
> micromachined it without any major issues?
> know of any suppliers?
>
> Thanking you in advance.
>
> Regards,
>
> Fred.
>
> --------------------------------------------
> Dr Fred Hussain
> The Technology Partnership plc
> Melbourn Science Park
> Cambridge Road
> Melbourn
> Royston
> Hertfordshire
> SG8 6EE
>
> Tel: 01763 262626
> Fax: 01763 261582
> www.ttpgroup.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
University Wafer
Mentor Graphics Corporation