MEMSnet Home: MEMS-Talk: Silicon Nitride Deposition ( PECVD or LPCVD)
Silicon Nitride Deposition ( PECVD or LPCVD)
2002-05-23
Javeed Shaikh Mohammed
2002-05-24
Robert M. Hamilton
2002-05-24
Kenneth Smith
Silicon Nitride Deposition ( PECVD or LPCVD)
Javeed Shaikh Mohammed
2002-05-23
Hello all,
         Iam a Graduate student looking for Process providers. I need to
deposit a Silicon Nitride layer of thickness 0.3-0.6 microns. I need residual
stress in the film to be TENSILE ( ranging 60-90 MPa). The Silicon nitride can
be either PECVD or LPCVD.

If anyone has some information, please mail me.

Javeed Shaikh Mohammed,
BIOMINDS LAB,IFM,
Louisiana Tech University.
Phone: (318) 257-5127
FAX:   (318) 257-5104
MAIL: PO Box 10307,911 Hergot Ave.
      Ruston, LA  71272

-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics