MEMSnet Home: MEMS-Talk: wet etch of Si with KOH
wet etch of Si with KOH
2002-05-30
Haigh, Richard
wet etch of Si with KOH
Haigh, Richard
2002-05-30
I have the following device structure PZT on Pt on Ti on SiO2 on Si with a
Si3N4 back face mask. Before etching in KOH The PZT is secured to a glass
plate with black wax, so as the face with the nitride mask will be etched.

During etching KOH got under the black wax and appears to have detached the
Ti/Pt from the SiO2. It is not clear if the etchant has reacted with the Ti or
with the SiO2. Has anyone else come across this before?  Would anyone
understand the chemistry involved.

Regards


Richard

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.