Hello Mlan,
My arsenal lists heated HCl/HNO3 3/1 for etching indium. I believe this is
also known as Aqua Regia.
I have used 45C H2O/HCl/HNO3 15/4/1 to etch ITO, so it may still work with
a little dilution. THen again, maybe not.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Battery is safe if not provoked." -- _Batteries in a Portable World_
----- BEGIN GEEK CODE BLOCK -----
Version 3.1
GE/S$ d- s:- a- C+ UL P L++ E- W+ N+@ !o K++ w !O M !V PS+ PE++(-) Y
PGP-- t++@ 5++ X R+ !tv b++ DI+ D G e++/*>++++/* h---/* r+++ y+++
------ END GEEK CODE BLOCK ------


On Fri, 31 May 2002, Milan Buncick wrote:

> Hi all,
>       Can someone please recommend an etch recipe for indium metal.
> Thanks,
> Milan
>
> Dr. Milan Buncick
> Director, MEMS/Photonics
> The AEgis TEchnologies Group Inc.
> 655 Discovery Drive
> Suite 301
> Huntsville, AL 35806
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group
MEMS Technology Review