Bonding microchannels using SU-8
2002-06-04
Mikkel Fougt Hansen
Bonding microchannels using SU-8
Mikkel Fougt Hansen
2002-06-04
Hi All

We would like to make microchannels using SU-8 for both the channel structures
(down to 10 microns) and the bonding. We will use either two glass wafers or a
pyrex wafer and a silicon wafer. Adhesion does not seem to be a problem. Can
you recommend a good procedure for bonding the two wafers, while maintaining
the channel structures?

We are aware of two options:

1) make and develop structures on one wafer, coat a second wafer with SU-8,
softbake and clamp (pressed by fingers) the wafers together at 75C, cool
slowly, expose to UV to crosslink, post-exposure baking

2) coat one wafer with SU-8, softbake and clamp to another wafer with
pre-drilled holes at 75C to bond, expose to UV,  post-exposure baking, develop
through drilled holes


Any help will be appreciated,

Mikkel Hansen

-------------------------------------------------------------------
Mikkel Fougt Hansen, Ph.D.
MIC - Microelectronics Centre
DTU, Oersteds Plads
Building 345E
DK-2800 Kgs. Lyngby
Denmark
Ph: (+45) 4525 6338
Fax: (+45) 4588 7762
E-mail [email protected]
http://www.mic.dtu.dk
-------------------------------------------------------------------

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review