MEMSnet Home: MEMS-Talk: SiN passivation problem
3. dielectric materials can survive HF
2002-05-31
Andrea Leppart
SiN passivation problem
2002-06-05
Robert Dean
2002-06-05
___
SiN passivation problem
Robert Dean
2002-06-05
>Hello,

I have a MEMS sensor that has aluminum traces covered with 0.4um of
silicon-nitride, for passivation, that must operate in a moist-salty
environment.  The part has failed, and I suspect that the moist-salty air
has permeated through the SiN layer and damaged the aluminum traces
underneath.  Any suggestions?


Robert Dean

Research Associate IV
Center for Advanced Vehicle Electronics
Auburn University
200 Broun Hall
Auburn, AL 36849

Voice: 334-844-1838
Fax:   334-844-1898
Email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.