2002-06-05
I am looking for a tape to put on the backside of 100 mm Si wafers to preserve
the oxide on the back, while etching the front in buffered oxide etch.

I have seen this done using dicing tape.  A coworker told me about something
called "Yellow Tape" that came in circular pieces the same size as the wafer,
apparently made for this purpose.  After use, the Yellow Tape was removed with
acetone, which would be an advantage over peeling dicing tape from delicate
substrates.

Could someone refer me to a source for this Yellow Tape or suggest an
alternative?

Roger Shile

"This email and any attachments may contain information that is confidential
and proprietary information of Veeco Instruments Inc. and are intended only
for the use of the addressee. Unauthorized use, distribution or copying is
forbidden. If you have received this email in error, please notify the sender
immediately by return email and delete all copies of this message and any
attachments from your computer. Thank you."

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Harrick Plasma, Inc.
University Wafer