A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to plasma etch Al?
How to plasma etch Al?
2002-06-10
lib zhou
2002-06-10
[email protected]
2002-06-10
[email protected]
Contact Lithography and Scanning
2002-07-07
Sreemanth M Venkata Uppuluri
How to plasma etch Al?
[email protected]
2002-06-10
To properly etch Al you will need a reactor with a load lock to prevent
moisture and also protect your operators from potentially dangerous
byproducts. That is because you will need to run a chemistry like BCL3 +
Chlorine to be able to etch through the Al2O3 that forms on the Aluminum then
a mixture of BCL3 and Chlorine with Argon or Helium to etch the bulk of the
Aluminum.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics