Greg Miller
2002-06-19
I've been working with SU-8 50 over the last year and things have been
working well -
However, recently I order a bottle of SU-8 they sent me the new 2000
series-
after I re-optimize the spin speed and followed there standard cure
process on silicon wafer - We still have adhesion problems or film
stress issue that do not occur with the old SU-8

I was wondering if anyone has run into this problem and could offer a
solution.

Thanks,

Greg Miller
KVH Industries
Email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.