MEMSnet Home: MEMS-Talk: wet etching and/or dry etching of Ni
wet etching and/or dry etching of Ni
2002-06-24
Xu Li
2002-06-24
Bigelow . Mike
wet etching and/or dry etching of Ni
Bigelow . Mike
2002-06-24
Ion milling will probably give you the
best results.

If you need this done, please contact me


-Mike

_______________
Mike Bigelow
Technical Sales

DRC - Metrigraphics
60 Concord Street
Wilmington, MA 01887   USA

Tel:  + (978) 658-6100  ext. 3063
Fax: + (978) 657-7765


-----Original Message-----
From: Xu Li [mailto:[email protected]]
Sent: Monday, June 24, 2002 4:58 AM
To: [email protected]
Subject: [mems-talk] wet etching and/or dry etching of Ni


Dear all,

Would anybody advice me how a straight and smooth side wall can be obtained
by
either wet or dry etching through a ~200nm Ni film?

Thank you very much in advance!

Xu Li
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review