Hi everyone,

I have the one problem which is happened in the etching chamber of PVD tools.
When I finished the etching process then I reload the nitride wafer, the wafer
will shift in the chamber.
If I using the oxide wafer, it will be fine.
Does any body talk to me what's force to make  the wafer moving?

Thanks,
Cairns

reply