A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: AZ4562 or other thick photoresist
AZ4562 or other thick photoresist
2002-07-02
hzeng
Problems with liftoff(on quartz)
2002-07-03
Balaji Lakshminarayanan
2002-07-03
A.J Pang
2002-07-03
Qingwei Mo
RE: AZ4562 or other thick photoresist
2002-07-05
hzeng
2002-07-08
Anatoli Olkhovets
2002-07-03
Grobe, Dirk
2002-07-08
Danny Hirdes
AZ4562 or other thick photoresist
Grobe, Dirk
2002-07-03
Hi Hongjun Zeng!

Try the AZ9260 photo resist, quite a bit better in aspect ratio and plasma
resistance, to be developed in AZ400K (best: 1:4) developer.
You can easily strip it with acetone.

But be aware: Only good for positive image. No image reversal possible. But
since your AZ45xx can't be reversed either, this might be the right resist for
you.

Regards
Dirk Grobe

----------------------------------------
Gesellschaft f|r Diamantprodukte mbH, Ulm
Company for Diamond Products Ltd., Ulm, Germany
  fon: +49(731)505-4546
  fax: +49(731)505-4561


> -----Original Message-----
> From: hzeng [mailto:[email protected]]
> Sent: Tuesday, July 02, 2002 10:12 PM
> To: [email protected]
> Cc: [email protected]; Hongjun Zeng
> Subject: [mems-talk] AZ4562 or other thick photoresist
>
>
> Dear Collegues,
>
> Could you help me to reach the answer of following questions,
>
> 1. Where can I get the AZ4562 photo resist, especially in US?
> 2. Is there any extreme thick photoresist else which can be
> easily removed by chemical liquid such as acetone?
>
> Thanks for your attention,
>
> Hongjun Zeng
> Microfabrication Applications Laboratory (MAL)
> University of Illinois at Chicago
> ERF Building, 842 W. Taylor Street
> Chicago, IL 60607-7022
> Room 3014 ERF
> Tel.: 312-413-5889, Fax: 312-996-6465
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change
> your list options, visit
> http://mail.mems-> exchange.org/mailman/listinfo/mems-talk
>
> Hosted by the MEMS
> Exchange, providers of MEMS processing services. Visit us at
http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review
Nano-Master, Inc.