SiO2 etching with 49% HF
Mighty Platypus
2002-07-15
Liviu,
According to "Etch Rates for Micromachining Processing" (JMEMS V.5,#4),
COncentrated HF will etch "wet" Thermal Oxide at between 18000 and 23000
A/min. "dry" oxide should be similar.
Are you considering etching the buried oxide layer on an SOI wafer to
release it?
Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"We did our best but God didn't want to give us any goals."
 -- Saudi Arabian goalkeeper Mohammed Al-Deayea (World Cup 2002)

On Mon, 15 Jul 2002, NICU Liviu wrote:

> Dear MEMS experts,
>
> I'm looking for details concerning the etching speed of thermal SiO2
(especially
> burried SiO2 specific to SOI wafers) by using 49% HF.
>
> Could you give me any references or brief informations about this?
>
> Thanks a lot,
>
> Liviu
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics