photosensitive glass
A.J Pang
2002-07-17
you can try http://www.mikroglas.com/foturane.htm

http://www.us.schott.com/tgd/english/products/foturan.html

http://www.darpa.mil/dso/thrust/md/chap/briefings/timchap2000day2/jacobsen_s
arcos.pdf

http://www.ee.ucla.edu/~jjudy/classes/ee250a/papers/Liu_SOG_MEMS_JMEMS.pdf

http://www.spike.cc/mikroglas.htm

http://ipewww.epfl.ch/gr_buttet/Manips/Nanotubes/papers/CNTpapers/Applicatio
ns/Wang_APL98.pdf

I think you need a UV light source and a high temperature oven (up to 700
deg)

cheers,

AJ Pang

----- Original Message -----
From: "Christopher J. Goetz" 
To: 
Sent: Wednesday, July 17, 2002 5:11 PM
Subject: [mems-talk] photosensitive glass


> Canyon Materials in San Diego (www.canyonmaterials.com) offers e-beam
> and laser sensitive glass which may be of interest to you. They also
> have access to corresponding exposure tools.
>
> C Goetz
>
> From: "Peng Jin" 
> To: 
> Date: Tue, 16 Jul 2002 12:59:02 +0100
> Subject: [mems-talk] About the Photosensitive glass
> Reply-To: [email protected]
>
> Dear fellow MEMS Researchers,
>
> In my experiment, I plan to use the photosensitive glass for high aspect
>
> ratio structure. I remember that there were some informtion about it.
> But I can not find it now.
>
> Could you provide some information about the supplier of this kind of
> thing. If there are somebody has done this before, could you tell which
> kind equipment is necessary for it?
>
> Any suggestion are highly appreciated.
>
> Cheers
>
> Peng
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

[demime 0.98e removed an attachment of type application/msword which had a name
of Photo glass.doc]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Addison Engineering
Mentor Graphics Corporation