Peng Yao
2002-07-22
Roger Shile
KOH etch stop
Roger Shile
2002-07-22
One micron of buried oxide should be more than sufficient as an etch "stop"
under these conditions.  I suggest that you measure the Si etch rate, then
calculate the time required to etch to the Si-SiO2 interface.  Allow for
some time for overetch, but not long enough to go through the oxide.

If you want to further improve the etch selectivity of the Si to SiO2, try
lowering the KOH concentration to 20% and the temperature to 70 degC.

Roger Shile

-----Original Message-----
From: Peng Yao [mailto:[email protected]]
Sent: Monday, July 22, 2002 6:13 AM
To: [email protected]
Subject: [mems-talk] KOH etch stop


Hi,
I planed to stop the KOH wet etching by the buried oxide layer of SOI
wafer. But every time when I did the experiment, KOH just etched through
the oxide layer. The oxide layer is about 1 micron thick, with 2 or 10
micron 100 silicon on top. According to some references, it should be equal
to 300-400 microns silicon in 30wt% KOH solution @80 degree. But everytime
I did the experiment, I just saw the reaction kept going and going, and
suddenly etch through the wafer. (By seeing the bubble of reaction. I
assume that the bubbling will decrease or even disappear when reaction
reached to the oxide)
Any explain or suggestion will be really appreciated.

Thanks a lot!

Peng Yao
DOEs lab
Electrical Engineering Dept.
Univeristy of delaware
Newark D.E 19716
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
"This email and any attachments may contain information that is confidential and
proprietary information of Veeco Instruments Inc. and are intended only for the
use of the addressee. Unauthorized use, distribution or copying is forbidden. If
you have received this email in error, please notify the sender immediately by
return email and delete all copies of this message and any attachments from your
computer. Thank you."

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Harrick Plasma, Inc.