Hello All,

I am working with SU8 and there is something i would like to try with
it, but i am not sure it is possible:
I would like to create SU 8 structures with sloped walls (as oppose to
vertical). Can we use a graded mask (from dark to light without steps)
for this? has anyone done it before?
If yes, are the results convincing?

Thanks a lot in advance for your help,

Magali Brunet
--
PEI Technologies,
NMRC, Lee Maltings, University College,
Cork, Ireland.

Tel: +353 21 4 904279
Fax: +353 21 4 270271
email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group
MEMStaff Inc.