Dear List,



Does anyone have a good recipe for etching MgO?  Specifically I have a
thin PZT film deposited on a 250mm MgO substrate.  I would like to
remove all of the substrate and collect the film for TEM analysis.



Best regards,



Jon Hiller



Jon M. Hiller

Argonne National Laboratory

Electron Microscopy Center

Materials Science Division

Tel:  630-252-9558

Fax:  630-252-4289

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing