MEMSnet Home: MEMS-Talk: Depth of oxidation into Aluminium thin films by oxygen plasma
Depth of oxidation into Aluminium thin films by oxygen plasma
2002-08-01
W.H. Teh
Depth of oxidation into Aluminium thin films by oxygen plasma
W.H. Teh
2002-08-01
Hi colleagues,

I have about 5nm of Alumnium thin film and I blast it with oxygen plasma
with an RF barrel asher...the end result shows a significantly higher
resistance, hence more oxidation has occurred (besides the native oxide on
the surface) , the question is how deep is the oxidation? Is the Al thin
film fully oxidized or not? What are the possible stochiometry of alumnium
oxide? Is there anyone out there who can share with me some of their
results on this? Thanks in advance!

Regards,
Weng

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
University Wafer
MEMS Technology Review