MEMSnet Home: MEMS-Talk: Depth of oxidation into Aluminium thin films by oxygen plasma
Depth of oxidation into Aluminium thin films by oxygen plasma
2002-08-01
[email protected]
Depth of oxidation into Aluminium thin films by oxygen plasma
[email protected]
2002-08-01
Weng:
I am not sure how much oxidation has occured on the surface of the wafer but
I would guess that no more than 500-1000 angstroms. That material is now
Al203 and very hard to etch. A significant amount of ion energy will be
required to etch the material in a plasma a high bias with BCL3 would do the
trick. Also most phosphoric acid based etchants will also etch the AL203 with
a little surfactant in the etchant for uniform breakthrough of the oxide. Bob
Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
University Wafer
The Branford Group