SPR-220 spin coating problem
2002-08-01
Mahesh Pitchumani
2002-08-01
Greg Miller
2002-08-01
Bill Moffat
SPR-220 spin coating problem
Greg Miller
2002-08-01
Mahesh -

This website has fairly good processing procedure for SPR220-7.0 -
http://www-snf.stanford.edu/Process/Lithography/SPR220.html
I use this as a guideline modified it alittle to optimize my process.

Thanks,

Greg Miller
KVH Industries
Email: [email protected]


-----Original Message-----
From: Mahesh Pitchumani [mailto:[email protected]]
Sent: Thursday, August 01, 2002 1:35 PM
To: [email protected]
Subject: [mems-talk] SPR-220 spin coating problem


Hi,

I am trying to spin coat SPR-220-7 thick resist from MicroChem with an
objective of getting 10-40 micron thick layers. I tried the process
supplied
by the company but it seems to give an uneven coat. Could anybody
suggest some
recipes for coating 10-40 micron thick layers with SPR_220.
I Thank you in advance for your help.


Mahesh Pitchumani
School of Optics/CREOL,
University of Central Florida.
4000 Central Florida Blvd,
Orlando, FL 32816-2700
Ph  : 407-823-6827
Fax : 407-823-6880
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation
Addison Engineering