I am looking for some piranha clean formulas.  SPS produces glass and quartz
wafers and we do not want to damage our surface finishes, yet we want to be
able to remove the microscopic traces that we have found.  Can someone
recommend a recipe that they have had good luck with?  Or perhaps a source for
multiple recipes that I could experiment with?

Any help would be appreciated.

Thank you,

Kris
Sensor Prep Services
704 E. North Street
Elburn, IL  60119
(630) 365-9645 phone
(630) 365-9643 fax
email: [email protected]
www.sensorprepservices.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
MEMStaff Inc.
Mentor Graphics Corporation