Aug. 4, 1995

I need a moldable material with which I can form disks that are 50 to 100 mm in
diameter and 0.5 to 1.0 mm thick (larger disks are the thicker). I need to be
able to impart microstructures into both sides with a minimum feature size of
0.7 to 1.0 micrometers square. I need a low coefficient of linear expansion
(this is the hard part) of about 5 x 10E-6 (10 times lower than acrylic). It
needs to be capable of taking an optically smooth finish and strong enough to
rotate at 3,600 to 7,200 rpm.

Any suggestions would be appreciated.

Thanks.

Steve Morton
Oxford Computer, Inc.
e-mail: [email protected]
http://www.fentonnet.com/oxford


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics