MEMSnet Home: MEMS-Talk: Nanoelectrodes suppliers
Nanoelectrodes suppliers
2002-08-09
Rakesh Dabas
2002-08-12
Kousik Sivakumar
2002-08-11
David Barrow
2002-08-12
Vic Kley
Nanoelectrodes suppliers
David Barrow
2002-08-11
Dear Rakesh
we can define nanoscale features with a minimum line width of 70nm using our
Raith direct write system. If you wish to send a sketch showing precise
geometries and list materials specifications (substrate, adhesion, electrode
material, thickness) we can give you some definitive feedback on how we can
help.
Cheers
David Barrow

-----------------------------------------------
Professor David Barrow
Laboratory for Applied Microsystems & NanoFAB
Cardiff School of Engineering
Cardiff University
Queen's Buildings
1-5 The Parade
PO Box 689
Cardiff CF24 3TF
Wales
United Kingdom
Tel   +44(0)29 2087 5921 (Office)
Tel   +44(0)29 2087 4716 (Laboratory)
Mob   +44(0)77 8526 4780
E-m   [email protected]
-----------------------------------------------

>>> [email protected] 08/09/02 16:09 PM >>>
Dear MEMS friends,
I tried to find out suppliers of nanoelctrodes on web,
& i also contact to some suppliers, but they can
fabricate only the microelectrodes (gap between
electrodes >5 micron). I want nanoelectrodes (gap
between nanoelectrodes should <200 nm). We have
facility for fabrication of microelectrodes. If
anybody can solve my problem then contact me on
address given below:
Rakesh Dabas
Scintist
Microelectronics Instrumentation Division (MID)
Central Scientific Instruments Organisation (CSIO)
Sector 30-C, Chandigarh-160030
India
E-Mail: [email protected]
        [email protected]


________________________________________________________________________
Want to sell your car? advertise on Yahoo Autos Classifieds. It's Free!!
       visit http://in.autos.yahoo.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering