MEMSnet Home: MEMS-Talk: Contamination issue of additive in THAH etching
Contamination issue of additive in THAH etching
2002-08-12
[email protected]
2002-08-12
Tabada, Phillipe
2002-08-13
Michael D Martin
Contamination issue of additive in THAH etching
Tabada, Phillipe
2002-08-12
Hi Grace,

   To give you a more accurate answer, you have to describe the type of
contamination.  Are they particulates, residue, etc?

Phil Tabada

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Monday, August 12, 2002 4:45 AM
To: [email protected]
Subject: [mems-talk] Contamination issue of additive in THAH etching


Hi all,
i am working on silicon anisotropic etching using TMAH recently,
in order to control the roughness of etched silicon and the selectivity to
Al and oxide,
we add silicic acid (SA) and ammonium persulfate (AP),
and as refer to S. Brida's recipe,
we add 2.5g AP per 15min to the etchant (~2L) to maintain the etching rate,
after 1~3 hours of etching,
we take the sample out the etchant,
and rinse it in DI water,
and there are plenty of contamination over the sample,
if anyone have any ideal or experience about how to avoid the contamination
issue,
many thanks,

Reference paper : S. Brida,"Microstructures etched in doped TMAH
solutions," Microelectronic Engineering, 53 (2000), 547-551

Grace Kuo
====================================
Global Communication Technology, Corp.
8F, No. 10, Prosperity Rd. 1 , SBIP,
Hsin Chu, Taiwan, R.O.C.
Tel : 886-3-5638686 ext . 7201
Fax : 886-3-5638432
E-Mail : mailto:[email protected]
====================================
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
DISCLAIMER: Unless expressly stated otherwise, this message is confidential
and may be privileged. It is intended for the addressee(s) only. Access,
copying, disclosure or re-use of the e-mail or any information contained
therein by any other person is not authorized. If you are not the intended
recipient please notify the sender immediately by returning the e-mail to the
originator.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group