Seems like a bit of a problem for coating in near vertical holes. You might
want to consider a company called Jet Process located in Ct. Their technology
is very low temperature for depositing oxide using their process. Contact
Dick Hart at 203-777-6000 and tell him Bob Henderson sent you. Bob

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics