Coducting Resin
2002-08-19
sanjay chakane
2002-08-20
Christopher F. Blanford
Coducting Resin
Christopher F. Blanford
2002-08-20
Try a silver-loaded epoxy. Two 10g vials cost 40 quid in the UK from RS
(rswww.com). It's a two-part epoxy that cures in 24h at room
temperature. It's a bit of a pain to work with, but it sticks well to
glass, metal, and plastic and has a nearly negligible resistivity (0.001
ohm cm). Chris

On Monday, August 19, 2002, at 08:11  pm, sanjay chakane wrote:

> Dear all
> If anybody knows conducting epoxy to join conducting
> materials which can be used at room temperature
> Sanjay
--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: (44)/(0)-1865-282603; Fax: (44)/(0)-1865-272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
University Wafer
Nano-Master, Inc.