A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Dissolving Gold electrodes
Dissolving Gold electrodes
2002-08-21
Jeroen Nieuwenhuis
2002-08-21
David Nemeth
2002-08-22
Heiko van der Linden
2002-08-22
Dr. Stefan Fiedler
2002-08-22
Christopher Blanford
2002-08-21
Tabada, Phillipe
2002-08-22
Nico Visch
Dissolving Gold electrodes
Tabada, Phillipe
2002-08-21
Hi Jeroen,

   What substrate and adhesion layer are you using for these gold
electrodes?

Phil

-----Original Message-----
From: Jeroen Nieuwenhuis [mailto:[email protected]]
Sent: Wednesday, August 21, 2002 9:30 AM
To: [email protected]
Subject: [mems-talk] Dissolving Gold electrodes


Dear all,

I am trying to measure the impedance of a 1% NaCl solution using 50 um x 150
um gold electrodes (thickness 0.6 um) in a microchannel and the electrodes
dissolve in about 40 minutes(!).

I used very pure NaCl and distilled water to make the solution. I use a
sine-wave generator to make a 50 mV AC voltage (offset oV) and I measure the
current using an transimpedance-amplifier with a 100k resistor. Nor the
source
nor the read-out electronics seems to generate a DC value current.

Does anybody have a suggestion what is going on? To the best of my knowledge
nothing should happen when the AC voltage used is less than about a volt.

Regards,
Jeroen Nieuwenhuis
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
DISCLAIMER: Unless expressly stated otherwise, this message is confidential
and may be privileged. It is intended for the addressee(s) only. Access,
copying, disclosure or re-use of the e-mail or any information contained
therein by any other person is not authorized. If you are not the intended
recipient please notify the sender immediately by returning the e-mail to the
originator.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.